Corrosion behavior of austenitic and ferritic steels in alkaline and water-salt solutions
DOI:
https://doi.org/10.15330/pcss.25.4.694-699Keywords:
corrosion tests, metallographic studies, sulfide corrosion, austenite, ferriteAbstract
The paper presents the results of studies of the corrosion behavior of austenitic and ferritic steels in alkaline, sulfide, and chloride environments. Structural changes on the surface when the steels are kept in solutions at room temperature are shown. The chemical composition of the steels was determined, and the exact phase-structural composition was theoretically predicted and metallographically determined. It was found that austenitic steel is almost not subject to sulfide corrosion at room temperature and chlorine-containing substances. At the same time, ferritic steel, under the same conditions, has significant corrosion damage on the surface, especially in places of mechanical damage.
References
C. Schwalm, M. Schütze, The corrosion behavior of several heat resistant materials in air +2 vol% Cl2 at 300 to 800 °C Part I - Fe base and Fe containing alloys, Materials and Corrosion, 51, 34 (2000); https://doi.org/10.1002/(SICI)1521-4176(200001)51:1<34::AID-MACO34>3.0.CO;2-0.
A. Schmid, G. Mori, R. Haubner, M. Weil, S. Hönig, Behaviour of S31400 and S32205 steels in HCl- and H2S- containing gas atmospheres under a low oxygen partial pressure between 480 and 680 °C, Materials and Corrosion, 69, 1 (2018); https://doi.org/10.1002/maco.201709992.
J. Yu, L. Sun, C. Ma, H. Yao, Thermal degradation of PVC: a review, Waste Management, 48, 300 (2016); https://doi.org/10.1016/j.wasman.2015.11.041.
A. Zahs, M. Spiegel, H.J. Grabke, The influence of alloying elements in the chlorine induced high temperature corrosion if Fe-Cr alloys in oxidizing atmospheres, Materials and Corrosion, 50, 561 (1999); https://doi.org/10.1002/(SICI)1521-4176(199910)50:10<561::AID-MACO561>3.0.CO;2-L.
J. Huanga, D. Yi, J. Yanb, B. Hanc, Y. He, Z. Yang, Y. Zhoub, F. Yang, Effects of Mn addition on oxidation behaviour of heat-resistant steel in a high-temperature steam environment, Corrosion Communications, 14, 72 (2024); https://doi.org/10.1016/j.corcom.2023.09.003.
G. Li, H. Xing, M. Du, M. Sun, L. Ma, Accelerated corrosion of 70/30 copper-nickel alloys in sulfide-polluted seawater environment by sulfide, Journal of Materials Research and Technology, 30, 8620 (2024); https://doi.org/10.1016/j.jmrt.2024.05.212.
B.D. Morton, H. Wang, R.A. Fleming, M. Zou, Nanoscale surface engineering with deformation - resistant core–shell nanostructures, Tribology letters, 42 (1), 51 (2011); https://doi.org/10.1007/s11249-011-9747-0.
M. Nimmervoll, G. Mori, S. Honig, R. Haubner, High-temperature corrosion of austenitic alloys in HCl and H2S containing atmospheres under reducing conditions. Corrosion Science, 200, 1102214 (2022); https://doi.org/10.1016/j.corsci.2022.110214.
M.O. Egbuhuzor, C.O. Akalezi, S.B. Ulaeto, D.I. Njoku, B.I. Onyeachu, E.E. Oguzie, Electro-deposited nanocomposite coatings and their behaviours against aqueous and high-temperature corrosion: A review, Hybrid Advances, 5, 1001180 (2024); https://doi.org/10.1016/j.hybadv.2024.100180.
W.T. Bakker, The effect of chlorine on mixedoxidant corrosion of stainless steel, Materials at High Temperatures, 14 (3), 197 (1997); https://doi.org/10.1080/09603409.1997.11689545.
V.A.C. Haanappel, N. Haanappel, T. Fransen, H.V. Corbach, P. Gellings, Corrosion kinetics of low- and high-alloy steels in chlorine-containing gas atmospheres, Corrosion, 48, 812 (1992); https://doi.org/10.5006/1.3315879.
E. Kordzadeh, M. Bozorgmehr, The effect of nickel increasing and aluminium addition on sulfidation resistance of Fe-Ni-Cr alloys, International Journal of Engineering, 21, 161 (2008).
J. Brown, D. Clark, W. Clark, Stability of the so-called delta ferrite-phase in austenitic steels, Journal of the Iron and Steel Institute, 174 (4) (1953).
Downloads
Published
How to Cite
Issue
Section
License
Copyright (c) 2024 Hanna Kniazieva, Sergey Kniaziev, Roman Tomashevskyi, Nadia Kanunnikova, Bohdan Vorobiov, Oleksii Shestopalov, Antonina Sakun
This work is licensed under a Creative Commons Attribution 3.0 Unported License.